ABSTRACT:
A ceramic igniter comprising: a) a lead wire, b) a ceramic substrate, and c) a braze pad having a thickness of less than about 150 microns, wherein the lead wire and ceramic substrate are placed in electrical connection by the braze pad.

REFERENCES:
patent: 3006069 (1961-10-01), Rhoads et al.
patent: 3779804 (1973-12-01), Urban
patent: 4122771 (1978-10-01), Barton et al.
patent: 4512871 (1985-04-01), Kato et al.
patent: 4521798 (1985-06-01), Baker
patent: 4544611 (1985-10-01), Rellick
patent: 4555358 (1985-11-01), Matsushita et al.
patent: 4818821 (1989-04-01), Wentworth et al.
patent: 4835344 (1989-05-01), Iyogi et al.
patent: 4883745 (1989-11-01), Mizuhara
patent: 5045237 (1991-09-01), Washburn
patent: 5085804 (1992-02-01), Washburn
patent: 5164246 (1992-11-01), Tanaka et al.
patent: 5367195 (1994-11-01), DiGiacomo et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Active metal metallization of mini-igniters by silk screening does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Active metal metallization of mini-igniters by silk screening, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Active metal metallization of mini-igniters by silk screening will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1239968

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.