ABSTRACT:
Described is an acidic glass fiber binding composition comprising an aqueous soluble phenol formaldehyde resin having low free formaldehyde, an effective amount of a formaldehyde scavenger, and an effective amount of a strong aqueous soluble acid, wherein the composition has an acidic pH and the solids content ranges from about 1 to about 30% by weight of the total composition. Also described is a method of binding glass fibers such as newly formed warm glass fibers at junctions of the fibers by applying the composition as described above to the fibers and then drying the composition. Also described are B-staged and C-staged glass fiber compositions having a alkylamine content less than 5 ppm.
REFERENCES:
patent: Re30375 (1980-08-01), Deuzeman et al.
patent: 2931738 (1960-04-01), Stalego
patent: 3072595 (1963-01-01), Bart et al.
patent: 3223668 (1965-12-01), Stalego
patent: 3253948 (1966-05-01), Tiede
patent: 3331885 (1967-07-01), Rider et al.
patent: 3487048 (1969-12-01), Deuzeman
patent: 3616179 (1971-10-01), McCombs et al.
patent: 3617428 (1971-11-01), Carlson
patent: 3702798 (1972-11-01), Shannon
patent: 3707296 (1972-12-01), Palazzolo et al.
patent: 3734918 (1973-05-01), Meger et al.
patent: 3817920 (1974-06-01), Lengager
patent: 3819441 (1974-06-01), Fargo et al.
patent: 3839236 (1974-10-01), Foley et al.
patent: 3907724 (1975-09-01), Higginbottom
patent: 3915905 (1975-10-01), Hanton
patent: 3919134 (1975-11-01), Higginbottom
patent: 3956204 (1976-05-01), Higginbottom
patent: 3956205 (1976-05-01), Higginbottom
patent: 4028367 (1977-06-01), Higginbottom
patent: 4060504 (1977-11-01), Higginbottom
patent: 4176105 (1979-11-01), Miedaner
patent: 4285848 (1981-08-01), Hickson
patent: 4324833 (1982-04-01), Yau
patent: 4576972 (1986-03-01), Lunt et al.
patent: 4611020 (1986-09-01), Bornstein et al.
patent: 4757108 (1988-07-01), Walisser
patent: 4960826 (1990-10-01), Walisser
Dornfeld Edmund G.
Mathews Dale J.
Miele Philip F.
Lusignan Michael
Quinn Cornelius P.
Schuller International, Inc.
LandOfFree
Acidic glass fiber binding composition, method of use and curabl does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Acidic glass fiber binding composition, method of use and curabl, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Acidic glass fiber binding composition, method of use and curabl will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-137444