Accelerated whisker growth on iron-chromium-aluminum alloy foil

Metal treatment – Process of modifying or maintaining internal physical... – Processes of coating utilizing a reactive composition which...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

502439, 148285, C23C 1108

Patent

active

049157515

ABSTRACT:
An accelerated method for growing oxide whiskers on aluminum-containing stainless steel foil comprises heating the foil in air at an initial temperature suitably less than 960.degree. C., preferably between 900.degree. C. and 950.degree. C., to initiate whisker growth and thereafter increasing the temperature to above 960.degree. C., preferably between 960.degree. C. and 990.degree. C., to continue whisker growth at an accelerated rate and thereby reduce the time and processing expense required to grow mature whiskers of a desired size.

REFERENCES:
patent: 4318828 (1982-03-01), Chapman
patent: 4331631 (1982-05-01), Chapman et al.
patent: 4414023 (1983-11-01), Aggen et al.
patent: 4588449 (1986-05-01), Sigler
patent: 4661169 (1987-04-01), Aggen et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Accelerated whisker growth on iron-chromium-aluminum alloy foil does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Accelerated whisker growth on iron-chromium-aluminum alloy foil, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Accelerated whisker growth on iron-chromium-aluminum alloy foil will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2297461

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.