ABSTRACT:
A process for making polyvinylpyrrolidone (PVP) K-90 having a polydispersity of less than 6, preferably less than 5, and most preferably, less than 4, which comprises polymerizing vinylpyrrolidone monomer by free radical solution polymerization, in water, in the presence of polyethylene glycol (PEG) having a molecular weight of about 300 as a chain transfer agent. The product is an aqueous solution of 15-25% PVP K-90, preferably 20%, 15-30% PEG, preferably 25%, and 45-70% water, preferably 55%, by weight of the solution.
REFERENCES:
patent: 4699146 (1987-10-01), Sieverding
Cullen James P.
Curry James F.
Wu Chi-San
Cheng Wu C.
ISP Investments Inc.
Katz Walter
Maue Marilyn J.
Schofer Joseph L.
LandOfFree
Process for making narrow molecular weight distribution polyviny does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for making narrow molecular weight distribution polyviny, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making narrow molecular weight distribution polyviny will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-952653