ABSTRACT:
Porous, adhesion-promoting oxide coatings are formed on titanium by anodizing in an aqueous solution containing fluoride ion and one or more oxidizing electrolytes at current densities of from 0.25 to 5 amp./ft..sup.2.

REFERENCES:
patent: 2829091 (1958-04-01), Missel et al.
patent: 3025225 (1962-03-01), Snyder et al.
patent: 3180807 (1965-04-01), Quinn
patent: 3198718 (1965-08-01), Quinn
patent: 3502552 (1970-03-01), Mizushima et al.
patent: 3616279 (1971-10-01), Kendall
"Ti Sandwich Panel R & D," Johnson et al., General Dynamics, Fort Worth, Tex., Final Report, AMC-59-7-618, Vol. 3, Contract No. AF33(600)-34392, Nov. 1959, pp. 5, 6, 109-110, 332-337.
"Anodizing Ti," H. Geduld, Metal Finishing, Apr. 1967, pp. 62-66.
"Adhesive Bonding of Ti & Its Alloys," NASA Tech. Memo., TMX-53313, Aug. 4, 1965, pp. 18-34.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of anodizing titanium to promote adhesion does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of anodizing titanium to promote adhesion, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of anodizing titanium to promote adhesion will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-903279

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.