Increasing the reactivity of coupling of block polymers

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

525375, 525379, 525382, 525384, 525385, 526173, 526336, C08F 840

Patent

active

043992609

ABSTRACT:
There is disclosed a process for the preparation of thermoplastic block polymers which comprises contacting conjugated diolefinic monomers selected from the group consisting of isoprene, piperylene, 2-ethyl-1,3-butadiene, 2,3-dimethyl-1,3-butadiene and 1,3-butadiene, and the like, mixed with at least one polyvinyl aromatic coupling compound selected from the group of o, m and p-divinylbenzene, 1,2,4-trivinylbenzene, 1,8-divinylnaphthalene, 1,2-divinyl-3,4-dimethylbenzene, 2,4-divinylbiphenyl, 3,5,4'-trivinylbiphenyl and 1,3,5-trivinylbenzene under solution polymerization conditions with a polystyryllithium catalyst which has been prepared by reacting an alkyllithium compound with a styrene monomer selected from the group consisting of styrene, alpha-methylstyrene, p-methylstyrene, p-t-butylstyrene, 3-methylstyrene, 1-vinylnaphthalene, and the like, in which an amount of polyvinyl aromatic coupling compound ranges from about 1.0 to about 6 vinyl groups of the polyvinyl aromatic coupling compound per mole of active lithium catalyst used, in which the living block copolymer is treated with (A) a polar compound selected from the group consisting of ethylene glycol dimethyl ether (glyme), diethylene glycol dimethyl ether (diglyme), triethylene glycol dimethyl ether (triglyme), tetraethylene glycol dimethyl ether tetraglyme), 2,3-dimethoxybutane, N,N,N',N'-tetramethylethylene-diamine (TMEDA), tri-n-butylphosphine and hexamethylphosphoric triamide (HMPA), in which the molar ratio of the said polar compounds to the active lithium ranges from about 0.01/1 to about 20/1 or (B) a polar compound selected from the group consisting of tetrahydrofuran, diethyl ether, triethylamine, 1,4-diazabicyclo-2.2.2-octane (DABCO), p-dioxane, tri-n-butylamine and N,N'-dimethylpiperazine, in which the molar ratio of the said polar compounds to the active lithium ranges from about 0.5/1 to about 100/1.

REFERENCES:
patent: 3363659 (1968-01-01), Keckler et al.
patent: 3639517 (1972-02-01), Kitchen et al.
patent: 3855189 (1974-12-01), Farrar et al.
patent: 3911054 (1975-10-01), Roest et al.
patent: 3931126 (1976-01-01), Naylor
patent: 3949020 (1976-04-01), Prudence
patent: 3951931 (1976-04-01), Burchard et al.
patent: 4163764 (1979-08-01), Nash
patent: 4304886 (1981-12-01), Bean, Jr. et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Increasing the reactivity of coupling of block polymers does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Increasing the reactivity of coupling of block polymers, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Increasing the reactivity of coupling of block polymers will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-815468

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.