Method for refining non-oxide ceramic powders

Plastic and nonmetallic article shaping or treating: processes – Including step of generating heat by friction

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

Other Related Categories

156635, 156646, 264344, C04B 3806

Type

Patent

Status

active

Patent number

049099736

Description

ABSTRACT:
A method for refining powders comprising the steps of: (a) adding polytetrafluoroethylene powders to non-oxide ceramic powders to form a mixture by mixing; and (b) heating the mixture in non-oxidizing atmosphere to convert oxides existing on the surface of the non-oxide ceramic powders into gaseous fluorides, and removing gaseous fluorides. The fluororesin is a polytetrafluoroethylene resin. The heating temperature in the non-oxidizing atmosphere is 500.degree. C. to 1300.degree. C.

REFERENCES:
patent: 4124665 (1978-11-01), Peterson et al.
patent: 4238434 (1980-12-01), Enomoto et al.
Brynestad et al, Communications of the American Ceramic Society, 1983, C-215 & 216.
Brynestad et al, Communications of the American Ceramic Society, 1984, C-184 & 185.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for refining non-oxide ceramic powders does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for refining non-oxide ceramic powders, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for refining non-oxide ceramic powders will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-791206

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.