ABSTRACT:
To produce electrolytic deposition of glossy gold/tin alloys there are employed baths having a pH below 3 which contain 1 to 20 g/l gold in the form of tetracyanoaurate (III), 0.1 to 10 g/l tin, an acid and a conducting salt, whereby the tin is in the form of a tin (IV)-oxalato complex.

REFERENCES:
patent: 3475290 (1969-10-01), Yamamura et al.
patent: 4013523 (1977-03-01), Stevens et al.
patent: 4069113 (1978-01-01), Crossley et al.
patent: 4391679 (1983-07-01), Zilske et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process and bath for the electrolytic deposition of gold-tin all does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process and bath for the electrolytic deposition of gold-tin all, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process and bath for the electrolytic deposition of gold-tin all will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-682762

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.