ABSTRACT:
A silica glass optical fiber is subjected to an external strain which causes vitreous matrix atoms to stabilize in a lower energy condition. In this way inhomogeneity domain sizes and as a consequence the attenuation due to Rayleigh scattering, depending on such inhomogeneity, are reduced.

REFERENCES:
patent: 3300288 (1967-01-01), Matthews
patent: 3912478 (1976-10-01), Precly
patent: 4447124 (1984-05-01), Cohen

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of reducing optical-fiber attenuation does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of reducing optical-fiber attenuation, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing optical-fiber attenuation will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-619265

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.