ABSTRACT:
A method of preparing a stainless steel surface for bonding by anodically treating the steel in an electrolytic bath, at a temperature of 60.degree. F to 180.degree. F, of an aqueous solution of sulfuric acid or an aqueous solution of sulfuric and chromic acids with an impressed voltage during anodizing of a range to remain within the passive region of the stainless steel.

REFERENCES:
patent: 2375210 (1945-05-01), Batcheller
patent: 3804730 (1974-04-01), Evans et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Preparing an environmentally stable stainless surface for bondin does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparing an environmentally stable stainless surface for bondin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparing an environmentally stable stainless surface for bondin will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-598155

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.