Method of making anisotropic magnets

Metal treatment – Process of modifying or maintaining internal physical... – Magnetic materials

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

419 12, 419 67, 419 41, 722531, 72700, B22F 300

Patent

active

049850857

ABSTRACT:
A process making anisotropic permanent magnets by extruding a neodymium-iron-boron alloy having a grain size of from 500.ANG. to 2000.ANG.at a temperature less than the melting temperature of the alloy at an extrusion ratio of from 10:1 to 26:1.

REFERENCES:
patent: 4374665 (1983-02-01), Koon
patent: 4402770 (1983-09-01), Koon
patent: 4496395 (1985-01-01), Crost
patent: 4585473 (1986-04-01), Narasimhan
patent: 4597938 (1986-07-01), Matsuura et al.
patent: 4601875 (1986-07-01), Yamamoto et al.
patent: 4684406 (1987-08-01), Matsuura et al.
"NdFeB Magnets Having a (100) Fiber Texture", B. M. Ma, R. F. Krause and V. K. Chandhok, Proceedings of the 9th International Workshop on Rare Earth Magnets and Their Application, Bad Soden, FRG, Aug. 31-Sept. 2, 1987-pp. 545-551.
"Radially Oriented NdFeB Magnets", Bao-Min Ma, V. K. Chandhok, and E. J. Dulis-1987 Digest of Intermag Conference, Tokyo, Japan, Apr. 14-17, 1987.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making anisotropic magnets does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making anisotropic magnets, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making anisotropic magnets will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-53247

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.