ABSTRACT:
A method of manufacturing a reflecting mirror is proposed which includes a double nickel layer plated on a stainless steel sheet as a base material. After buffing, the base material is immersed in a 4 to 9% solution of hydrochloric acid to remove any oxide thereon, thus performing a pre-treatment step. The method also features a pre-plating step which forms an initial plated nickel layer on the surface of the base material, using a bath composition comprising 150 to 300g/l of nickel chloride and 3.6 to 36g/l of hydrochloric acid. The method also includes a bright nickel plating step which employs a standard Watts bath.

REFERENCES:
patent: 915415 (1909-03-01), Cowper-Coles
patent: 2285548 (1942-06-01), Wesley
patent: 2557823 (1951-06-01), Holbrook
patent: 2878172 (1959-03-01), Scavullo
patent: 3186925 (1965-06-01), Kushner
patent: 3338803 (1967-08-01), Di Bari

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing a reflecting mirror does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing a reflecting mirror, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing a reflecting mirror will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-486508

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.