ABSTRACT:
Repair of compressor blades (6) of aircraft engines is performed by build-up welding against an essentially horizontal backing (8) whose surface shape is the exact negative of the respective bottom side of the blade to be repaired. With low rework effort, the blades of blisks can, in the installed state, be repaired or fully restored at any point with high quality upon removal of the damaged portion.

REFERENCES:
patent: 3777106 (1973-12-01), Nuccel
patent: 4195475 (1980-04-01), Verdouw
patent: 4237361 (1980-12-01), Zwintscher et al.
patent: 4246463 (1981-01-01), Shutt et al.
patent: 4509673 (1985-04-01), Schmidt et al.
patent: 4726104 (1988-02-01), Foster et al.
patent: 4775092 (1988-10-01), Edmonds et al.
patent: 4832252 (1989-05-01), Fraser
patent: 4841117 (1989-06-01), Koromzay
patent: 4842663 (1989-06-01), Kramer
patent: 5038014 (1991-08-01), Pratt et al.
patent: 5067234 (1991-11-01), Fraser
patent: 5147999 (1992-09-01), Dekumbis et al.
patent: 5165758 (1992-11-01), Howe
patent: 5235745 (1993-08-01), Fraser
patent: 5261480 (1993-11-01), Wortmann et al.
patent: 5321228 (1994-06-01), Krause et al.
patent: 5553370 (1996-09-01), Pepe
patent: 5701669 (1997-12-01), Meier
patent: 5913555 (1999-06-01), Richter et al.
patent: 6049979 (2000-04-01), Nolan et al.
patent: 6172327 (2001-01-01), Aleshin et al.
patent: 6198187 (2001-03-01), Asao et al.
patent: 6238187 (2001-05-01), Dulaney et al.
patent: 6326585 (2001-12-01), Aleshin et al.
patent: 6468367 (2002-10-01), Mukira et al.
patent: 6469271 (2002-10-01), McGoey
patent: 6580959 (2003-06-01), Mazumder
patent: 6607114 (2003-08-01), Reser et al.
patent: 6754955 (2004-06-01), Carl et al.
patent: 2002/0015654 (2002-02-01), Das et al.
patent: 2003/0042233 (2003-03-01), Kelly
patent: 003813157 (1988-12-01), None
patent: 3942051 (1990-08-01), None
patent: 4032615 (1992-04-01), None
patent: 19547903 (1997-03-01), None
patent: 19642980 (1998-08-01), None
patent: 19957771 (2001-06-01), None
patent: 0403736 (1990-12-01), None
patent: 60115370 (1985-06-01), None
patent: 361069424 (1986-04-01), None
patent: 09314364 (1997-12-01), None
patent: 10308472 (1998-11-01), None
patent: 02001025863 (2001-01-01), None
Metals Handbook, “Superalloys; Processing”, 12 pages, 2002.
IBM Technical Disclosure Bulletin; NB930633; “Thermal Control of High Powere Devices During Card/Circuit Test”; Jun. 1, 1993.
ASM Handbooks Online; Controlling Heat Effects; 1 page; copyright 2003.
ASM Handbooks Online; Mitigation of Intergranular SCC in BWR Piping; sub heading “Heat Sink Welding”; pp. 1-3; copyright 2003.
German Search Report dated Dec. 2, 2003.
European Search Report dated Jul. 15, 2004.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for the restoration of damaged areal components does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for the restoration of damaged areal components, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the restoration of damaged areal components will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4021198

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.