ABSTRACT:
A soft magnetic film is formed which is represented by the formula (FexNiy)aMob, in which 0.65≦x≦0.75 and x+y=1 are satisfied when x and y are on a mass percent ratio basis, and 0<b≦5 and a+b=100 are satisfied when a and b are on a mass percent basis, and by using this soft magnetic film, a lower core layer and/or an upper core layer is formed. Accordingly, a saturated magnetic flux density of 1.6 T or more and a resistivity of 40 μΩ·cm or more can be obtained, and hence a thin film magnetic head having a small loss in a high frequency signal region can be provided.
REFERENCES:
patent: 4242710 (1980-12-01), Hempstead et al.
patent: 4536229 (1985-08-01), Jin et al.
patent: 5935346 (1999-08-01), Couderchon et al.
patent: 6183881 (2001-02-01), Shimizu
patent: 6262867 (2001-07-01), Sano et al.
patent: 6376108 (2002-04-01), Otagiri et al.
patent: 6449122 (2002-09-01), Yazawa et al.
patent: 2002/0154444 (2002-10-01), Sano et al.
patent: 63-100148 (1988-02-01), None
patent: 8-212512 (1996-08-01), None
patent: 9-63016 (1997-03-01), None
patent: 2000-58364 (2000-02-01), None
patent: 2000-235911 (2000-08-01), None
Kanada Yoshihiro
Yazawa Hisayuki
Alps Electric Co. ,Ltd.
Brinks Hofer Gilson & Lione
Sheehan John P.
LandOfFree
Soft magnetic film and thin film magnetic head using the same does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Soft magnetic film and thin film magnetic head using the same, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Soft magnetic film and thin film magnetic head using the same will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-3649972