ABSTRACT:
A process comprises depolymerizing, with 1,4-butane diol, a first polymer comprising a polyethylene terephthalate component in the presence of at least one second polymer selected from the group consisting of polyvinyl chlorides, polyvinylidene chlorides, polyamides, polylactic acid, and combinations thereof to produce a molten mixture; and polymerizing the molten mixture under conditions sufficient to form a modified polybutylene terephthalate copolymer. The modified PBT comprises (a) at least one polyethylene terephthalate component residue, and (b) a member selected from the group consisting of (i) the at least one second polymer selected from the group consisting of polyvinyl chlorides, polyvinylidene chlorides, polyamides, polylactic acid, and combinations thereof; (ii) the at least one residue derived from the second polymer; and (iii) combinations thereof.
REFERENCES:
patent: 2465319 (1949-03-01), Whinfield et al.
patent: 2720502 (1955-10-01), Caldwell
patent: 2727881 (1955-12-01), Caldwell et al.
patent: 2822348 (1958-02-01), Haslam
patent: 3047539 (1962-07-01), Pengilly
patent: 3907868 (1975-09-01), Currie et al.
patent: 3953394 (1976-04-01), Fox et al.
patent: 3953404 (1976-04-01), Borman
patent: 4128526 (1978-12-01), Borman
patent: 4609680 (1986-09-01), Fujita et al.
patent: 5266601 (1993-11-01), Kyber et al.
patent: 5413681 (1995-05-01), Tustin et al.
patent: 5451611 (1995-09-01), Chilukuri et al.
patent: 5559159 (1996-09-01), Sublett et al.
patent: 6162837 (2000-12-01), Gerking et al.
patent: 6384129 (2002-05-01), Lowry
patent: 6410607 (2002-06-01), Ekart et al.
patent: 6444283 (2002-09-01), Turner et al.
patent: 6515044 (2003-02-01), Idel et al.
patent: 6518322 (2003-02-01), West
patent: 6706843 (2004-03-01), Ishihara et al.
patent: 6794463 (2004-09-01), Aramaki et al.
patent: 6887909 (2005-05-01), Kawamura et al.
patent: 6927275 (2005-08-01), Hirokane et al.
patent: 7179869 (2007-02-01), Hirokane et al.
patent: 7183362 (2007-02-01), Hirokane et al.
patent: 7388067 (2008-06-01), Leemans et al.
patent: 7462649 (2008-12-01), Nakao et al.
patent: 2002/0012807 (2002-01-01), Kurian et al.
patent: 2007/0203253 (2007-08-01), Agarwal et al.
patent: 2007/0208160 (2007-09-01), Agarwal et al.
patent: 2007/0244242 (2007-10-01), Agarwal et al.
patent: 2007/0275242 (2007-11-01), Gopal et al.
patent: 2007/0276069 (2007-11-01), Agarwal et al.
patent: 0683201 (1995-11-01), None
patent: 1500577 (1978-02-01), None
patent: 2000-256472 (2000-09-01), None
patent: 2002060369 (2000-09-01), None
patent: 2005-89572 (2005-04-01), None
patent: 20010083551 (2001-09-01), None
patent: 03066704 (2003-08-01), None
patent: 2007/089598 (2007-08-01), None
Pawlak, A.; Pluta, M.; Morawiec, J.; Galeski, A.; Pracella, M.; European Polymer Journal, 2000, 36, p. 1875-1884.
International Search Report; International Application No. PCT/US2007/002197; International Filing Date: Jan. 26, 2007; Date of mailing: Jun. 19, 2007; 5 pages.
S.H. Mansour et al.,“Depolymerization of Poly(ethylene terephthalate) Waste Using 1, 4-Butanediol and Triethylene Glycol,” Journal of Elastomers and Plastics; Apr. 2003, pp. 133-147, vol. 35, Sage Publications.
S. Sivaram et al., “Synthesis Characterization and Polycondensation of Bis-(4-Hydroxybutyl) Terephthalate,” Polymer Bulletin 5, 1981, pp. 159-166, Springer-Verlag.
ASTM Designation: D 790-03, “Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials,” pp. 1-11 (2003).
International Standard: ISO 178, “Plastics—Determination of Flexural Properties,” 23 pgs. (2001).
International Standard: ISO 1133, “Plastics—Determination of the Melt Mass-Flow Rate (MFR) and the Melt Volume-Flow Rate (MVR) of Thermoplastics,” pp. 1-16 (2005).
International Standard: ISO 11443, “Plastics—Determination of the Fluidity of Plastics Using Capillary and Slit-Die Rheometers,” pp. 1-34 (2005).
International Search Report and Written Opinion; International Application No. PCT/US2009/069079; International Filing Date Dec. 21, 2009; Applicant's file reference P090124PCT; Date of Mailing May 4, 2010; 13 pages.
“GE Gives Plastic Bottle Recycling a New Spin”; ChemicalProcessing.com, Aug. 25, 2006 [online], accessed via the internet [retrieved on Oct. 16, 2009], URS: <http://www.chemicalprocessing.com/industrynews/2006/056.html>; 2 pages.
Cantor & Colburn LLP
Jones, Jr. Robert
Sabic Innovative Plastics IP B.V.
Wu David
LandOfFree
Process for the manufacture of polybutylene terephthalate... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for the manufacture of polybutylene terephthalate..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the manufacture of polybutylene terephthalate... will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2765560