ABSTRACT:
Disclosed herein is a method for the production of an anisotropic magnetic powder or a magnet produced from said powder, wherein a hydrogenating and dehydrogenating method is applied to the starting material in order to produce the powder. An anisotropic oriented magnetic material, more particularly magnetic scrap metal, is advantageously used as starting material so that the complicated use of a molten mass with isotropic distribution of the c axes of the hard metal crystals is not required. The result is an anisotropic material having a fine grain structure and a crystallographic orientation matching a TMXB phase formed during hydrogenation.

REFERENCES:
patent: 4981532 (1991-01-01), Takeshita et al.
patent: 5049208 (1991-09-01), Yajima et al.
patent: 5091020 (1992-02-01), Kim
patent: 5110374 (1992-05-01), Takeshita et al.
patent: 5228930 (1993-07-01), Nakayama et al.
patent: 5314548 (1994-05-01), Panchanathan et al.
patent: 5580396 (1996-12-01), Fruchart et al.
patent: 5993732 (1999-11-01), Nakayama et al.
patent: 6149861 (2000-11-01), Kaneko et al.
patent: 6290782 (2001-09-01), Sakurada et al.
patent: 6444052 (2002-09-01), Honkura et al.
patent: 2002/0059965 (2002-05-01), Honkura et al.
patent: 2003/0209294 (2003-11-01), Honkura et al.
patent: 2005/0067052 (2005-03-01), Honkura et al.
patent: 693 15 807 (1994-05-01), None
patent: 197 47 364 (1998-05-01), None
patent: 197 51 367 (1999-06-01), None
patent: 198 43 883 (1999-10-01), None
patent: 199 50 835 (2001-05-01), None
patent: 0 924 720 (1999-06-01), None
patent: 1 191 553 (2002-03-01), None
patent: 61-179803 (1986-08-01), None
patent: 06-151130 (1994-05-01), None
patent: 10-032113 (1998-02-01), None
patent: 2002-105503 (2002-04-01), None
patent: 2002-161302 (2002-06-01), None
patent: 2002-180211 (2002-06-01), None
patent: 2002-237406 (2002-08-01), None
ASM Materials Engineering Dictionary, 1992, p. 211.
Gutfleisch, et al., ‘Texture Inducement During HDDR Processing of NdFeB,’IEEE Transaction on Magnetics, 38(5):2958-2960 (2002).
Japanese Notification of Reasons for Refusal issued on Aug. 11, 2009.
Japanese Office Action dated Aug. 27, 2010 for Japanese Application No. 2004-554511.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for the production of an anisotropic magnetic powder... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for the production of an anisotropic magnetic powder..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for the production of an anisotropic magnetic powder... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2737743

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.