ABSTRACT:
The invention relates to a weld filler and to a use of a weld filler which significantly improves the weldability of some nickel-based superalloys and includes the following constituents (in wt %): 17.5%-20.0% chromium (Cr) 10.0%-12.0% cobalt (Co) 9.0%-10.5% molybdenum (Mo) 0.1%-3.3% titanium, in particular 3.0%-3.3% titanium (Ti), 1.4%-1.8% aluminum (Al), 0.04%-0.12% carbon, 0.003%-0.01% boron (B), remainder nickel.

REFERENCES:
patent: 3741824 (1973-06-01), Duvall et al.
patent: 4219592 (1980-08-01), Anderson et al.
patent: 4359352 (1982-11-01), Ray et al.
patent: 6024792 (2000-02-01), Kurz et al.
patent: 6702906 (2004-03-01), Ogawa et al.
patent: 6797232 (2004-09-01), Speidel et al.
patent: 2004/0115086 (2004-06-01), Chabenat et al.
patent: 2006/0051234 (2006-03-01), Pike
patent: 2006/0144477 (2006-07-01), Cox et al.
patent: 0 412 397 (1991-02-01), None
patent: 0 486 489 (1992-05-01), None
patent: 0 786 017 (1997-07-01), None
patent: 0 892 090 (1999-01-01), None
patent: 1 204 776 (2002-05-01), None
patent: 1 306 454 (2003-05-01), None
patent: 1 319 729 (2003-06-01), None
patent: 1 428 897 (2004-06-01), None
patent: WO 99/67435 (1999-12-01), None
patent: WO 00/44949 (2000-08-01), None
K. Banerjee, N.L. Richards, M.C. Chaturvedi; “Effect of Filler Alloys on Heat-Affected Zone Cracking in Preweld Heat-Treated IN-738 LC Gas-Tungsten-Arc Welds”, Metallurgical and Materials Transactions A; Jul. 2005; pp. 1881-1890, vol. 36A; XP009059582.
E.F. Bradley; “Superalloys A Technical Guide”; ASM International; 1988; Chapter 13; pp. 197-199, 201, 207, 212-214, 13; XP002361607; Metals Park, Ohio, US.
Ramazan Kayacan, Remzi Varol, Olcay Kimilli; “The effects of pre- and post-weld heat treatment variables on the strain-age cracking in welded Rene 41 components”; Materials Research Bulletin 39 . . . 11, 2004, pp. 2171-2186, XP004607869; Pergamon Press, New York, US.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Weld filler, use of the weld filler and welding process does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Weld filler, use of the weld filler and welding process, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Weld filler, use of the weld filler and welding process will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2690453

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.