ABSTRACT:
A method for manufacturing a tire carcass includes the step of providing a liner of an air-impermeable material. A carcass ply material is prepared by heating and stretching plastic cords and embedding the stretched plastic cords in rubber. A ply of the carcass ply material is placed onto the liner with overlapping leading and trailing ply ends. The overlapping ply ends are heated for returning the stretched plastic cords into an unstretched state. Bead cores are then positioned onto the ply. The lateral edges of the ply are folded over the bead cores. The folded lateral edges and the bead cores are then enveloped by lateral strips.

REFERENCES:
patent: 4261393 (1981-04-01), Saito et al.
patent: 5200009 (1993-04-01), Tokita
patent: 5437751 (1995-08-01), Hirano et al.
patent: 5616198 (1997-04-01), Suzuki et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for manufacturing a tire carcass to prevent sidewall cons does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for manufacturing a tire carcass to prevent sidewall cons, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for manufacturing a tire carcass to prevent sidewall cons will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2425632

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.