ABSTRACT:
This invention relates to the production of chemical pitch by stripping under reduced pressure steam cracker tar to obtain a pitch having an initial boiling point of between 350.degree. C and 400.degree. C at atmospheric pressure, heat soaking the pitch at 360.degree. to 420.degree. C in the absence of air or oxygen at sub-atmospheric to 4 atmospheres absolute and stripping under reduced pressure the soaked pitch to obtain a product having a minimum softening point (R and B) of 75.degree. C. This pitch can be mixed with coke to make electrodes especially suitable for aluminium production.

REFERENCES:
patent: 2848424 (1958-08-01), Stanko
patent: 3238116 (1966-03-01), Hamner et al.
patent: 3324029 (1967-06-01), King et al.
patent: 3725240 (1973-04-01), Baum
patent: 3970542 (1976-07-01), Bongertman
patent: 4017378 (1977-04-01), Fauveau et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Pitch bonded carbon electrode does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Pitch bonded carbon electrode, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pitch bonded carbon electrode will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2419763

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.