Process for producing polyurethane elastomer by mixing a hardene

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – From reactant having at least one -n=c=x group as well as...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

528 63, 528 64, C08G 1810

Patent

active

043272045

ABSTRACT:
A polyurethane elastomer is produced by mixing a hardener composition containing a polyamine, a long chain polyol having an average molecular weight of 300 to 4,000 and a catalyst with an isocyanate composition comprises a prepolymer having terminal isocyanate group and an average molecular weight of 500 to 5,000 and an organic diisocyanate monomer with or without a triisocyanate monomer and a ratio of isocyanate groups of said prepolymer to amino groups of said polyamine is in a range of 0.6:1 to 1.5:1 and a ratio of a total of isocyanate groups in said isocyanate composition to a sum of amino groups of said polyamine and hydroxyl group of said long chain polyol is in a range of 0.8:1 to 1.4:1.

REFERENCES:
patent: 3718624 (1973-02-01), Rustad
Wyman, Rubber World, May, 1978, pp. 41-44.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing polyurethane elastomer by mixing a hardene does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing polyurethane elastomer by mixing a hardene, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing polyurethane elastomer by mixing a hardene will most certainly appreciate the feedback.