Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...
Patent
1984-04-05
1987-07-21
Schofer, Joseph L.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
5253323, C08F 820
Patent
active
046819215
ABSTRACT:
Improved halogenated butyl rubbers are prepared by isomerizing the polymers so that a significant mole fraction of the halogen is in the primary allylic position. The isomerization is carried out utilizing as a catalyst either a Friedel Crafts catalyst or HBr.
REFERENCES:
patent: 3099644 (1963-07-01), Parker et al.
patent: 3816371 (1974-06-01), Baldwin et al.
patent: 3919131 (1975-11-01), Malatesta et al.
patent: 3965213 (1976-06-01), Baldwin et al.
patent: 4145492 (1979-03-01), Gardner
patent: 4288575 (1981-09-01), Gardner
Baldwin Francis P.
Fusco James V.
Gardner Irwin J.
Exxon Research & Engineering Co.
Lipman Bernard
Schofer Joseph L.
LandOfFree
Process for preparing improved halogenated butyl rubber does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for preparing improved halogenated butyl rubber, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing improved halogenated butyl rubber will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-207847