ABSTRACT:
A process for preparing a fully hydrolyzed polyvinyl alcohol modified melamine-formaldehyde resin useful in decorative laminates is disclosed. The process comprises reacting melamine, formaldehyde, and fully hydrolyzed polyvinyl alcohol at 80.degree.-90.degree. C. until the reaction product has a water tolerance of about 300% to 1000% in 5.degree. C. water. The mole ratio of melamine to formaldehyde is from about 1:1.5 to about 1:1.8, respectively.

REFERENCES:
patent: 3458465 (1969-07-01), Rehnelt et al.
patent: 4138445 (1979-02-01), Nogi et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for the preparation of a fully hydrolyzed polyvinyl alco does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for the preparation of a fully hydrolyzed polyvinyl alco, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for the preparation of a fully hydrolyzed polyvinyl alco will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1916134

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.