ABSTRACT:
The dimensions of a plastic product are controlled while injection molding the product in a mold cavity of a mold comprising a core section and a cavity section, separated by a parting line and defining the mold cavity. In one method the mold cavity wall thicknes is controlled during an injection of a first quantity of plastic material by locking the core section to impede lateral movement thereof by means of contact between a non-perpendicular contact surface of a protracted contact element of one mold section and an associated non-perpendicular contact surface of the other mold section, and is further controlled during an injection of a second quantity of plastic material, which occurs a predetermined period after discontinuing the flow of plastic material into the mold cavity and after the contact element has been retracted, by locking the core section to impede lateral movement thereof by means of a at-least-partly-solidified wall sections having a controlled thickness formed during the injection of the first quantity of plastic material. In another method, the mold cavity wall thickness is controlled during an injection of a first quantity of plastic material, which does not completely cover the parting line of the mold, by locking the core section to impede lateral movement thereof by means of contact between a non-perpendicular contact surface of a protracted contact element of one mold section and an associated non-perpendicular contact surface of the other mold section, and is further controlled during an injection of a second quantity of plastic material, which occurs after the contact element has been retracted, by locking the core section to impede lateral movement thereof by means of at-least-partly-solidified wall sections having a controlled thickness formed during the injection of the first quantity of plastic material.

REFERENCES:
patent: 3305892 (1967-02-01), Heider
patent: 3737272 (1973-06-01), Segmuller
patent: 4339408 (1982-07-01), Jenkins
patent: 4508676 (1985-04-01), Sorensen
patent: 4733801 (1988-03-01), Scammell

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Injection-molding product wall-thickness control methods does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Injection-molding product wall-thickness control methods, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Injection-molding product wall-thickness control methods will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1885443

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.