ABSTRACT:
A high-strength, tough alloy steel is formed by heating an alloy steel comprising iron, 0.1-0.4 weight % carbon, 1-3 weight % manganese and 1-13 weight % chromium and optionally containing microalloying amounts of other metals to about 1150.degree. C. to form a stable homogeneous austenite phase, control rolling the steel at about 900.degree. C.-1100.degree. C., followed by rapid cooling to 950.degree. C. and again rolling at that temperature and then quenching the thusly rolled steel in liquid or by air cooling. Tempering at temperatures up to about 300.degree. C. may be effected to further increase the toughness of the steel.

REFERENCES:
patent: 3385740 (1968-05-01), Braggstrom et al.
patent: 4170497 (1979-10-01), Thomas et al.
patent: 4533401 (1985-08-01), Yutori et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of forming high-strength, tough, corrosion-resistant stee does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of forming high-strength, tough, corrosion-resistant stee, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of forming high-strength, tough, corrosion-resistant stee will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1826987

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.