Process for making polyvinylpyrrolidone polymer having predeterm

Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

526212, C08F12610, C08F 204

Patent

active

053628152

ABSTRACT:
A process for making a solution of PVP K-90 polymer having a weight average molecular weight, Mw, of about 630,000 to 750,000 and a molecular weight distribution, Mw/Mn, where Mn is the number average molecular weight of the polymer, of 5 or less, which comprises free radical polymerizing about 5-30% by weight vinylpyrrolidone, preferably 10-20%, at about 40.degree.-100.degree. C., preferably 60.degree.-75.degree. C., in an aqueous-alcohol solvent selected from the group consisting of about (a) 5% isopropanol-95% water, (b) 10% ethanol-90% water and (c) 20% methanol-80% water.

REFERENCES:
patent: 4520180 (1985-05-01), Barabas et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Process for making polyvinylpyrrolidone polymer having predeterm does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making polyvinylpyrrolidone polymer having predeterm, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making polyvinylpyrrolidone polymer having predeterm will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1783325

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.