Method of producing low core losses in oriented silicon steels

Metal treatment – Process of modifying or maintaining internal physical... – Magnetic materials

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 27, 148 28, H01F 104

Patent

active

046665358

ABSTRACT:
A method is provided for improving core-loss values of grain-oriented silicon steel after final texture annealing by boronizing the steel to levels of 0.001 to 0.009 wt. % after applying a boron-containing material to the final texture annealed steel, heating to 1850.degree. to 2200.degree. F., maintaining the steel at such temperature to infuse boron into other steel, and cooling the steel at a rate of 100.degree. F./hour or less.

REFERENCES:
patent: 3207636 (1965-09-01), Wada et al.
patent: 3670278 (1972-06-01), Foster et al.
patent: 3700506 (1972-10-01), Tanaka et al.
patent: 3905842 (1975-09-01), Grenoble
patent: 4096000 (1978-06-01), Wada et al.
patent: 4096001 (1978-06-01), Arendt et al.
patent: 4116730 (1978-09-01), Arendt et al.
patent: 4160681 (1979-07-01), Miller, Jr.
patent: 4179315 (1979-12-01), Miller, Jr.
patent: 4200477 (1980-04-01), Datta et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing low core losses in oriented silicon steels does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing low core losses in oriented silicon steels, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing low core losses in oriented silicon steels will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1562442

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.