Two step electrochemical etch process for high volt aluminum ano

Chemistry: electrical and wave energy – Processes and products – Electrostatic field or electrical discharge

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

20412975, C25F 304

Patent

active

045184712

ABSTRACT:
Aluminum electrolytic capacitor anode foil of a high cubic texture is etched using a two step process by treating the foil in an electrolyte bath containing 3% hydrochloric acid and 1% aluminum as aluminum chloride under the influence of a direct current of high current density and at a temperature of 75.degree. C., and in a second step treating said etched foil in a similar bath with a much lower current density and at a temperature of 80.degree. to 82.5.degree. C. The foil thus etched has a significantly higher capacitance resulting from a greater density of tunnels, and a fairly linear tunnel structure.

REFERENCES:
patent: 4213835 (1980-07-01), Fickelscher
patent: 4420367 (1983-12-01), Tocher

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Two step electrochemical etch process for high volt aluminum ano does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Two step electrochemical etch process for high volt aluminum ano, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Two step electrochemical etch process for high volt aluminum ano will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1536767

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.