ABSTRACT:
According to a method of molding a glass body, a glass preform is placed between upper and lower molds of a mold assembly. The mold assembly is then heated to a predetermined heating temperature falling within a heating temperature range corresponding to a glass viscosity range of the glass preform of 10.sup.8 to 10.sup.10.5 poise. A pressure high enough to mold the glass preform is applied between the upper and lower molds when the glass preform is at the predetermined heating temperature, so that an unfinished glass molded body is formed. The pressure is released, and the unfinished glass molded body and the mold assembly are gradually cooled to a temperature within a glass viscosity range of 10.sup.11.5 to 10.sup.14 poise while the unfinished glass molded body is held in the mold assembly. A glass molded body is then released from the mold assembly.

REFERENCES:
patent: 4398935 (1983-08-01), Smulders et al.
patent: 4435200 (1984-03-01), Joorman et al.
patent: 4591373 (1986-05-01), Sato et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of molding glass body does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of molding glass body, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of molding glass body will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1192948

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.