ABSTRACT:
Loom components such as reed dents or weft brake lamellae that, during operation, are exposed to frictional abrasion by a moving weft thread, are made of cold rolled strip steel or of refined nitrided steels. The components are then exposed to a heat treatment at a temperature larger than 480.degree. C. for a duration of more than two hours, preferably up to 8 hours. A thermo-chemical treatment is performed simultaneously with the heat treatment to harden at least those surface areas of the components that in operation will be exposed to the frictional abrasion.

REFERENCES:
patent: 5226975 (1993-07-01), Denton
German Industrial Standard (DIN) Handbook No. 155 "Quality Standards for Steel and Iron No. 2", 1985, pp. 119 and 120, published by Beuthverlag GmbH Berlin and Cologne, Second Edition (DIN 17 224).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method for increasing the surface hardness of loom components ex does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method for increasing the surface hardness of loom components ex, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method for increasing the surface hardness of loom components ex will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1101808

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.