ABSTRACT:
Prior to welding, a base metal of an austenitic stainless steel alloy is cooled to approximately -78.degree. C. This process, using a conventional filler metal, reduces microfissuring in welds.

REFERENCES:
patent: 2288068 (1942-06-01), Brebeck
patent: 3597833 (1971-08-01), Frederick et al.
patent: 4101067 (1978-07-01), Sloan et al.
patent: 4152568 (1979-05-01), Yamaguchi
patent: 4209123 (1980-06-01), Jay
patent: 4218604 (1980-08-01), Masaoka
patent: 4296300 (1981-10-01), Bottiglia

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of reducing microfissuring in welds having an austenitic does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of reducing microfissuring in welds having an austenitic , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing microfissuring in welds having an austenitic will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-110043

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.