ABSTRACT:
Preparation of the silica and alumina matrix components of a zeolite cracking catalyst while intimately mixing at a pH of 3.0 to about 4.5 results in a selective catalyst of high density and low pore volume. The coke produced during cracking emits lower amounts of sulfur during regeneration of tha catalyst translating to reduced sulfur oxide stack emissions.

REFERENCES:
patent: 2872410 (1959-02-01), Erickson
patent: 3124541 (1964-03-01), Wilson, Jr. et al.
patent: 3137658 (1964-06-01), Drake et al.
patent: 3313594 (1967-04-01), Wilson, Jr.
patent: 3451947 (1969-06-01), Michael
patent: 3520828 (1970-07-01), Rosinski
patent: 3531397 (1970-09-01), Michalko
patent: 3556988 (1971-01-01), Stover et al.
patent: 3939058 (1976-02-01), Plank et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing a high-density cracking catalyst with reduce does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing a high-density cracking catalyst with reduce, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing a high-density cracking catalyst with reduce will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1091631

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.