Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Mixing of two or more solid polymers; mixing of solid...
Patent
1980-09-15
1981-12-29
Levin, Stanford M.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Mixing of two or more solid polymers; mixing of solid...
525286, 525289, 525296, 525297, 525306, 525307, 526 73, C08F 202
Patent
active
043083609
ABSTRACT:
In a process for the mass polymerization of vinyl aromatic monomer wherein vinyl aromatic monomer is polymerized in successive stages of increasing temperature, the improvement which narrows the molecular weight distribution of the resulting polymer comprising incorporating a crosslinking agent into a polymerizing mass at a point where about 60 to about 95% of monomer is converted to polymer.
REFERENCES:
patent: 3919354 (1975-11-01), Moore et al.
patent: 3945976 (1976-03-01), McCurdy et al.
Levin Stanford M.
Magidson William H.
McClain William T.
Oliver Wallace L.
Standard Oil Company (Indiana)
LandOfFree
Process for obtaining narrow molecular weight distribution in vi does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for obtaining narrow molecular weight distribution in vi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for obtaining narrow molecular weight distribution in vi will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1019040